Service Report Lab number PAK-AWF-0813-572
Date 06-08-13
Customer Nazir Dyeing Karachi
For the attention of
Reference Mr Izhar Ul Haq
Subject Evaluation of durability of RUCOFIN GSQ 200 and GSP 200 after 10HL
Material 100% cotton towel
Trial parameters and profile
SOP
Towel treated with below mentioned recipe and procedure.
L: R 1:10Temperature 40˚CTime 30min
Trial 1 2 Unit
RUCOFIN GSQ 200 1 - %OWFRUCOFIN GSP 200 - 1Acetic acid pH 4-5 - -
Home Laundering It is carried out acc. to AATCC 135 with tide detergent at 40˚C.
RESULTS: treated and untreated, before wash and after wash all samples are attached for evaluation. After 10HL treated sample remained soft showing wash durability of softener.
RegardsFinishing /Textile LabRudolf PakistanTel: +92 425311591 Fax: +92 4235311530 E-mail: ghulam.jaffar@rudolf.pk
www.rudolf-group.com www.silverplus.com www.bionic-finish.com www.innovations-for-textiles.com
RUDOLF GmbH page 2 Lab number / 17.04.2023 / Initials