Ferolite NAM 39® Aeroilite 111® Ferolite Steel® Ferolite NAM 42 GF® Ferolite Special® Aerolite 1000® Max. Peak Temperature 250°C 380° C 415° C 440° C 550° C 600° C Internal Pressure limit 50 bar 35 bar 80 bar 150 bar 150 bar 200 bar Color Green/White/ Red/Yellow Green/Blue/ Red Gray/ Graphited White/Green Gray/Gray Gray/ Graphited Thickness (mm) 0.25 - 5 0.4-6 0.8-6 0.4-6 0.6-6 0.6-6 Physical properties Standard Unit Value Value Value Value Value Value Density (Nominal) DIN 28 090 [g/cm³] 1.15 - 1.90 1.15-1.90 1.8-2.1 1.7-2.00 1.7-2.2 1.7-2.2 Tensile Strength (a) Across Grain ASTM F152 [N/mm²] 7 ≥5 ≥10 ≥7 ≥24 ≥26 (b) Across Grain DIN52910 [N/mm²] Compressibility ASTM F 36A [%] 7 - 15 7 - 15 6 - 14 6 - 12 6 - 14 6 - 14 Recovery ASTM F 36A [%] 40 40 40 50 40 40 Fluid absorption In ASTM oil no.3 ASTM F 146 Increase in mass [%] 12 15 Increase in thickness [%] 10 13 15 In fuel B ASTM F 146 Increase in mass [%] 10 10 Increase in Thickness [%] 10 10 16 In water/antifreeze ASTM F 146 Increase in mass [%] 15 15 12 15 10 Increase in Thickness [%] 5 5 5 5 5 5 Ignition loss DIN 52911 [%] 40 40 35 30 28 26 STRESS RESISTANCE (16h 175°C) DIN 52913 [N/mm²] 10 10 17 30 23 26 General Information

کاتالوگ کلی ورقهای کلینگریت

Embed Size (px)

DESCRIPTION

a

Citation preview

  • Ferolite NAM 39 Aeroilite 111 Ferolite Steel Ferolite NAM 42 GF Ferolite Special Aerolite 1000

    Max. Peak Temperature 250C 380 C 415 C 440 C 550 C 600 C

    Internal Pressure limit 50 bar 35 bar 80 bar 150 bar 150 bar 200 bar

    ColorGreen/White/

    Red/Yellow

    Green/Blue/

    RedGray/ Graphited White/Green Gray/Gray

    Gray/

    Graphited

    Thickness (mm) 0.25 - 5 0.4-6 0.8-6 0.4-6 0.6-6 0.6-6

    Physical properties Standard Unit Value Value Value Value Value Value

    Density (Nominal) DIN 28 090 [g/cm] 1.15 - 1.90 1.15-1.90 1.8-2.1 1.7-2.00 1.7-2.2 1.7-2.2

    Tensile Strength

    (a) Across Grain ASTM F152 [N/mm] 7 5 10 7 24 26

    (b) Across Grain DIN52910 [N/mm]

    Compressibility ASTM F 36A [%] 7 - 15 7 - 15 6 - 14 6 - 12 6 - 14 6 - 14

    Recovery ASTM F 36A [%] 40 40 40 50 40 40

    Fluid absorption

    In ASTM oil no.3 ASTM F 146

    Increase in mass [%] 12 15

    Increase in thickness [%] 10 13 15

    In fuel B ASTM F 146

    Increase in mass [%] 10 10

    Increase in Thickness [%] 10 10 16

    In water/antifreeze ASTM F 146

    Increase in mass [%] 15 15 12 15 10

    Increase in Thickness [%] 5 5 5 5 5 5

    Ignition loss DIN 52911 [%] 40 40 35 30 28 26

    STRESS RESISTANCE (16h

    175C)DIN 52913 [N/mm] 10 10 17 30 23 26