Norwegian Oil and Gas Association Recommended Guidelines for NDT of GRP pipe systems and tanks No.: 055 Established: 01.03.97 Revision no: Date revised: Page: 3 ANNEX A A1 DRAFT PRACTICE FOR CLASSIFYING VISUAL DEFECTS IN GLASS-REINFORCED PLASTIC PIPES AND TANKS A.1 SCOPE A1 A.1.1 Pipe A1 A.1.2 Tanks A1 A.2 MAIN DETECTABLE DEFECTS A1 A.3 DEFECT TYPES AND ACCEPTANCE CRITERIA A2 A.3.1 Defect descriptions and assessment schedule A2 A.3.2 Acceptence criteria/ASTM/ D 2563 modifications A50 A.4 AREAS FOR FURTHER DEVELOPMENT A52 A.5 DRAFT INSPECTION PROCEDYRE A52 A.6 REFERENCES A54 ANNEX B B1 PRESSURE TESTING B.1 MAIN DETECTABLE DEFECTS B1 B.2 LIMITS OF DETECTABILITY B1 B.3 GENERAL B1 B.4 TEST PROCEDURE B1 ANNEX C C1 ULTRASONICS TEST METHODS AND DETECTABLE DEFECTS C.1 MAIN DETECTABLE DEFECTS C1 C.2 LIMITS OF DETECTABILITY C1 C.3 GENERAL C3 C.4 AREAS FOR FURTHER DEVELOPMENT C4 C.5 DRAFT INSPECTION PROCEDUREFOR ULTRASONIC INSPECTION OF ADHESIVELY BONDED FIBRE GLASS PIPE JOINTS C4 1.0 SCOPE C4 2.0 GENERAL REQUIREMENTS C4 3.0 EQUIPMENT C5 4.0 CALIBRATION C5 4.1 Calibration standard C5

055 - Guidelines for NDT of GRP Pipe Systems and Tanks 4

Embed Size (px)

DESCRIPTION

Page 4

Citation preview

  • Norwegian Oil and Gas Association Recommended Guidelines for NDT of GRP pipe systems

    and tanks

    No.: 055 Established: 01.03.97 Revision no: Date revised: Page: 3

    ANNEX A A1

    DRAFT PRACTICE FOR CLASSIFYING VISUAL DEFECTS IN

    GLASS-REINFORCED PLASTIC PIPES AND TANKS

    A.1 SCOPE A1

    A.1.1 Pipe A1

    A.1.2 Tanks A1

    A.2 MAIN DETECTABLE DEFECTS A1

    A.3 DEFECT TYPES AND ACCEPTANCE CRITERIA A2

    A.3.1 Defect descriptions and assessment schedule A2

    A.3.2 Acceptence criteria/ASTM/ D 2563 modifications A50

    A.4 AREAS FOR FURTHER DEVELOPMENT A52

    A.5 DRAFT INSPECTION PROCEDYRE A52

    A.6 REFERENCES A54

    ANNEX B B1

    PRESSURE TESTING

    B.1 MAIN DETECTABLE DEFECTS B1

    B.2 LIMITS OF DETECTABILITY B1

    B.3 GENERAL B1

    B.4 TEST PROCEDURE B1

    ANNEX C C1

    ULTRASONICS TEST METHODS AND DETECTABLE DEFECTS

    C.1 MAIN DETECTABLE DEFECTS C1

    C.2 LIMITS OF DETECTABILITY C1

    C.3 GENERAL C3

    C.4 AREAS FOR FURTHER DEVELOPMENT C4

    C.5 DRAFT INSPECTION PROCEDUREFOR ULTRASONIC

    INSPECTION OF ADHESIVELY BONDED FIBRE GLASS

    PIPE JOINTS C4

    1.0 SCOPE C4

    2.0 GENERAL REQUIREMENTS C4

    3.0 EQUIPMENT C5

    4.0 CALIBRATION C5

    4.1 Calibration standard C5