Atomic Layer Depositionfor Microchannel Plates
Jeffrey Elam
Argonne National Laboratory
September 24, 2009
Atomic Layer Deposition (ALD)
Layer-by-layer thin film coating method Atomic level control over thickness and composition Precise coatings on 3-D objects Deposit nearly any material (oxides, nitrides, metals, etc.)
Example:ALD Zinc Oxide in
deep trenches
Large Area Photodetector
Microchannel Plate (MCP)
– Electron amplifier (x104-107)
3
Microchannel Plates (MCPs)
Conventional Fabrication:– Draw glass fiber bundle– Slice and polish– Chemical etch, heat in hydrogen
Problems:– Expensive– Resistance and secondary emission properties are linked– Long conditioning process needed– Thermal runaway
4
ALD for Fabrication of MCPs
Start with porous, insulating substrate
– Glass capillary plate
– Anodic aluminum oxide (AAO) membrane ALD of resistive film on all surfaces (inside of pores, on faces, etc.) ALD of secondary electron emissive film Deposit metal electrodes on outer surfaces
5
33 mm
MCP Structure
6
1) resistive coating (ALD)2) emissive coating (ALD)3) conductive coating (thermal
evaporation or sputtering)
pore
ALD for Resistive Coating
Target: 10-100 MΩ through MCP ZnO: conductor Al2O3: insulator
ZnO/ Al2O3 alloy – tunable resistivity
Tune composition and thickness of film to adjust MCP resistance
7
ALD for Emissive Coating
8
Many material possibilities Tune SEE along pore
SiO2Al2O3
MgO
ZnO
Cross-Sectional Elemental Maps of ALD MCP
9
Zn
SEM Si
Al Au
ALD ZnO and Al2O3 extend into pores
Sputtered Au only on edge of pores
Glass capillary plate ALD ZnO/Al2O3
Sputter gold electrodes
Cross-Sectional Image of ALD Film in MCP
10
ALD Film
100 nm ALD film visible in middle of MCP
Glass
Questions?