Page 1: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Atomic Layer Depositionfor Microchannel Plates

Jeffrey Elam

Argonne National Laboratory

September 24, 2009

Page 2: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Atomic Layer Deposition (ALD)

Layer-by-layer thin film coating method Atomic level control over thickness and composition Precise coatings on 3-D objects Deposit nearly any material (oxides, nitrides, metals, etc.)

Example:ALD Zinc Oxide in

deep trenches

Page 3: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Large Area Photodetector

Microchannel Plate (MCP)

– Electron amplifier (x104-107)

3

Page 4: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Microchannel Plates (MCPs)

Conventional Fabrication:– Draw glass fiber bundle– Slice and polish– Chemical etch, heat in hydrogen

Problems:– Expensive– Resistance and secondary emission properties are linked– Long conditioning process needed– Thermal runaway

4

Page 5: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

ALD for Fabrication of MCPs

Start with porous, insulating substrate

– Glass capillary plate

– Anodic aluminum oxide (AAO) membrane ALD of resistive film on all surfaces (inside of pores, on faces, etc.) ALD of secondary electron emissive film Deposit metal electrodes on outer surfaces

5

33 mm

Page 6: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

MCP Structure

6

1) resistive coating (ALD)2) emissive coating (ALD)3) conductive coating (thermal

evaporation or sputtering)

pore

Page 7: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

ALD for Resistive Coating

Target: 10-100 MΩ through MCP ZnO: conductor Al2O3: insulator

ZnO/ Al2O3 alloy – tunable resistivity

Tune composition and thickness of film to adjust MCP resistance

7

Page 8: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

ALD for Emissive Coating

8

Many material possibilities Tune SEE along pore

SiO2Al2O3

MgO

ZnO

Page 9: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Cross-Sectional Elemental Maps of ALD MCP

9

Zn

SEM Si

Al Au

ALD ZnO and Al2O3 extend into pores

Sputtered Au only on edge of pores

Glass capillary plate ALD ZnO/Al2O3

Sputter gold electrodes

Page 10: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Cross-Sectional Image of ALD Film in MCP

10

ALD Film

100 nm ALD film visible in middle of MCP

Glass

Page 11: Atomic Layer Deposition for Microchannel Plates Jeffrey Elam Argonne National Laboratory September 24, 2009

Questions?

11