Time and Temperature of Eva Film Glass Laminating Inside Furnace Peter Lin It is unsuitable to process different kinds of glass or Dry Melt adhesive EVA Interlayer Film in the same stove with the same technique, otherwise it's difficult to guarantee the quality. Normally, the processing temperature for colored Dry Melt adhesive EVA Interlayer Film is a little higher than that for normal clear Dry Melt adhesive EVA Interlayer Film; the processing temperature for thick Dry Melt adhesive EVA Interlayer Film or glass is also a little higher than that for thin Dry Melt adhesive EVA Interlayer Film or glass; the processing temperature for laminated glass with interlayer silk is slightly higher than that for laminated glass only with EVA interlayer film. If the temperature is not suitable to be too high suddenly, we can extend the heat preserving time so as to increase temperature gradually. The appropriate processing period is based on the structure of the stove and the heating power. Customers may know more abut this after more practice. We suggest customers contact us for more information if customers are not sure about how to produce new laminated products or use new Dry Melt adhesive EVA Interlayer Films, in this way, the unnecessary loss or waste will be reduced.

Time and temperature of eva film glass laminating inside furnace

Embed Size (px)

Citation preview

Page 1: Time and temperature of eva film glass laminating inside furnace

Time and Temperature of Eva Film Glass Laminating Inside Furnace

Peter Lin

It is unsuitable to process different kinds of glass or Dry Melt adhesive EVA Interlayer Film inthe same stove with the same technique, otherwise it's difficult to guarantee the quality.

Normally, the processing temperature for colored Dry Melt adhesive EVA Interlayer Film is alittle higher than that for normal clear Dry Melt adhesive EVA Interlayer Film;the processing temperature for thick Dry Melt adhesive EVA Interlayer Film or glass is also alittle higher than that for thin Dry Melt adhesive EVA Interlayer Film or glass; the processingtemperature for laminated glass with interlayer silk is slightly higher than that for laminatedglass only with EVA interlayer film.

If the temperature is not suitable to be too high suddenly, we can extend the heat preservingtime so as to increase temperature gradually. The appropriate processing period is based onthe structure of the stove and the heating power.

Customers may know more abut this after more practice. We suggest customers contact usfor more information if customers are not sure about how to produce new laminatedproducts or use new Dry Melt adhesive EVA Interlayer Films, in this way, the unnecessaryloss or waste will be reduced.

Page 2: Time and temperature of eva film glass laminating inside furnace

All rights reserved by CNC GLASS INTERLAYER TECH:Product 1]CNC EVA FILM INERLAYER FOR ARCHITECTURAL LAMINATED [email protected] 2]CNC PDLC SMART GLASS FILM FOR PRIVACY SWITCHABLE [email protected] 3]CNC PVB FILM INTERLAYER FOR AUTOMOTIVE WINDSHIELD GLASSwww.cncglass.com