SX Superalloys For Turbine Blades Characterization ... · deviation from the [001] orienta- t ion...
13
SX Superalloys For Turbine Blades Characterization ... · deviation from the [001] orienta- t ion (within the limit of about 150 ) have any effect on the alloy. strength creep Conversely,